110℃ High-shrink-ratio Polyolefin Tubing

 

MATERIAL:Polyolefin, Shrink ratio: 3:1。 600V 
Operating temperature: -55 ℃ ~125 ℃ , Minimum shrink temperature : 70 ℃ ; 
Minimum fully recovery temperature : 110 ℃ ,
COLOR:BLACK--BK、RED--RD、BLUE--BL、YELLOE-Y、WHITE--W、GREEN--G, 
           Other colors on Requrest.
Features:flame-retardant, high-shrink-ratio irradiated crosslinking heat-shrinkable modified polyolefin tubing. 
Application:It is used for insulation protection, bundling or capsule of wire terminals and components with larger size differences.
Unit:mm

Part No.
As supplied
After recovery
L
ID
T
(max.) ID
T
(m/spool)
UHS-110-3X-0.5-BK
1.8±0.2
0.20±0.05
0.5
0.50±0.10
200
UHS-110-3X-1-BK
3.3±0.3
1
0.60±0.10
UHS-110-3X-2-BK
6.5±0.3
2
0.70±0.10
100
UHS-110-3X-3-BK
9.5±0.4
0.30±0.06
3
0.80±0.15
UHS-110-3X-4-BK
12.5±0.4
4
0.85±0.15
UHS-110-3X-6-BK
18.5±0.5
6
1.00±0.150
50
UHS-110-3X-8-BK
26.0±1.0
0.40±0.10
8
1.20±0.20
UHS-110-3X-13-BK
41.5±1.0
13
1.20±0.20

 

Property

items

Chemical
Test method
Typical data
Physical

Axial Shrinkage

5% max.
ASTMD2671
≤5%
Concentricity
70% min.
ASTMD2671
≥70%
Tensile strength
10.4MPa min.
ASTMD638
≥14.0MPa
Elongation
200% min
ASTMD638
≥400%
Heat shock
250℃, 4hrs
No cracking
ASTMD2671
Pass
Low temperature flexibility
-55℃, 4hrs
No cracking
ASTMD2671
Pass
Aging   158℃,168hrs
Tensile strength after aging
70% of original min.
ASTMD638
≥90%
Elongation after aging
100% min.
ASTMD638
≥300%
Electrical
Dielectric voltage withstand
2500V,60sec,no breakdown
UL224
Pass

Dielectric strength

19.7KV㎜ min.
ASTMD2671
25KV/mm

Volume resistivity

1014Ω·㎝ min.
ASTMD876
≥1014Ω·㎝
Chemical
Corrosion
No corrosion
ASTMD2671
Pass

Copper stability

Elongation ≥100%
ASTMD2671
Pass
Flammability
VW﹣1
UL224
Pass
Copyright 2009 - 2012 Shanghai Kinglok Electrical Material Co.,Ltd. All rights reserved.
Addr:Building 3,No. 380,Minmin Road,Pudong,Shanghai,China
Tel :+86 21-58381118,58991538,58350020,50478011 Fax :+86 21-50211732 E-mail: [email protected]