125°C Fourfold Shrink Ratio Polyolefin Tube

 

MATERIAL:Polyolefin ;  Shrinkage ratio 4:1 ;Shrink Temperature  90℃~125℃;Temperature Range  125 ℃;Radial Shrinking Ratio≥50% ;Longitudinal Shrinking Ratio≤15%;Tensile Strength≥10.4MPa;Elongation Ratio≥200%;Flammability:VW—1 
COLOR:BLACK--BK, Other Colors on Requrest.
Unit:mm

Part No.
Size
As supplied
After recovery
mm

ID

T

ID"(Max.)

T"(Min.)

UHS-125-4X-8
Ф8.0/2.0 
8.5±0.5 
0.30±0.15 
2.00
0.95±0.15 
UHS-125-4X-10
Ф10.0/2.5 
10.5±0.5 
0.30±0.15 
2.50
1.00±0.15 
UHS-125-4X-12
Ф12.0/3.0 
12.5±0.5 
0.30±0.15 
3.00
1.00±0.15 
UHS-125-4X-16
Ф16.0/4.0 
16.5±0.5 
0.30±0.15 
4.00
1.00±0.15 
UHS-125-4X-18
Ф18.0/4.5 
18.5±0.5 
0.30±0.15 
4.50
1.00±0.15 
UHS-125-4X-20
Ф20.0/5.0 
20.5±0.5 
0.30±0.15 
5.00
1.00±0.15 
UHS-125-4X-20
Ф25.0/6.25 
25.5±0.5 
0.40±0.20 
6.25
1.40±0.20 
Copyright 2009 - 2012 Shanghai Kinglok Electrical Material Co.,Ltd. All rights reserved.